The three hardness scales: HRC (Rockwell C, hard materials 20 to 70 HRC), HB (Brinell, soft to medium-hard, 450 HBW or below), HV (Vickers, full range, thin layer / micro area). Approximate conversion: HB is about 10 x HRC (accurate in the HRC 40 to 50 range, e.g. HRC40 about 390 HB, HRC50 about 500 HB); HV is about HB (with Brinell ball diameter 10 / 3000); HRC and HV can be roughly estimated by HRC about (HV - 150) / 11. For precision use the conversion table (GB/T 1172) or curve interpolation, as materials differ. Common correspondence see tb-146; for heat-treatment process see tb-145. (Note: material and process should match the service: parts under impact and wear suit quenching-tempering + surface hardening or carburizing; precision no-grind parts use nitriding. Welded structures prefer Q235 / low-alloy steel (good weldability), avoiding high-carbon steel cracks. For process temperature, microstructure and hardness correspondence see the process table tb-145 and hardness-conversion table tb-146.)