E41-482 · Motor Selection · Repaired Motor Insulation Treatment · ★★★★
The motor (55kW) suffered a turn-to-turn short circuit 30 minutes into the trial run after rewinding. On disassembly the winding ends were poorly impregnated, with gaps between the coils.
When the motor was repaired the stator winding was rewound and impregnated by dipping (dipping method, 4h impregnation). However the varnish used had too high a viscosity (200mm²/s, standard ≤100mm²/s) and poor flow, so it could not fully penetrate the small gaps between the coils (about 0.1~0.2mm). After baking and curing, gaps remained between the coils that had not been filled with varnish (void content about 15%). Under electromagnetic vibration (100Hz, amplitude about 0.01mm) fretting occurs between the coils, and the insulation layer on the enamelled wire (polyester-imide, about 0.05mm thick) is worn through, so bare copper touches bare copper → turn-to-turn short circuit. The heat generated by the short-circuit current melts the insulation of the neighbouring coils, the short circuit spreads and the motor protection trips. VPI was not used during the repair, so the insulation quality is below that of the original manufacture.
1) After rewinding the motor, vacuum pressure impregnation (VPI) should be used (vacuum degassing plus pressure impregnation, 100% varnish penetration)
2) Control the varnish viscosity: ≤100mm²/s (at 25℃) for good flow
3) Fit insulating spacers between the coils (Nomex paper, 0.25mm thick) to prevent direct contact
4) After impregnation check the insulation resistance (500V megohmmeter, ≥500MΩ)
5) Perform a dielectric withstand test (2×Un+1000V, 1min, no breakdown)
FT_12_Motor Selection Systematization