E41-011 · Ballscrew Selection · Stamping Auto-Feed Mechanism · ★★★
After about 8 months of operation the ballscrew fatigued and fractured at the nut-connection thread, causing the feed mechanism to crash and damaging the die. The fracture surface showed a typical fatigue appearance (shell marks + fast-fracture zone); the initial crack started at the thread-root stress concentration.
Ballscrew diameter d = 20 mm, dynamic load rating Ca = 15 kN, actual average axial load Fa = 8 kN, load ratio Fa/Ca = 53%. But stamping feed is a frequent-reversing impact duty (60 cycles/min); the impact factor K = 2.0 gives equivalent dynamic load Feq = K × Fa = 16 kN, exceeding Ca (15 kN). Also the screw thread root has a sharp-corner transition (no large fillet R0.5 mm), with stress-concentration factor Kt = 3.5, greatly reducing fatigue life. Calculated life L = (Ca/Feq)³ × 50 km = (15/16)³ × 50 km ≈ 41 km; at 0.5 m travel per minute this is only about 57 days.
① Check dynamic load rating: Ca/Feq ≥ 2 (including impact factor), Feq = K × Fa
② Increase diameter: choose d = 32 mm (Ca = 35 kN, Ca/Feq = 35/16 = 2.2 ✓)
③ Thread-root optimization: use a large fillet R ≥ 0.5 mm to reduce stress concentration
④ Material strengthening: use high-strength alloy steel (40CrMo or 50CrVA), quench + medium-temperature temper
⑤ Periodic lubrication: replenish grease every 500 h to reduce wear and fretting fatigue
FT_11 Ball Screw Selection