E41-191 · Screw Selection · Chemical Equipment Screw · ★★★
The chemical-equipment screw nut seal ring swelled and cracked after 1 month of use; grease leaked, and chemical gas entered the screw interior through the seal breach and corroded the raceway.
The screw grease was a general-purpose lithium grease, and the nut seal ring was NBR nitrile rubber (oil-resistant). But a small amount of benzene-type organic vapor (about 200ppm) existed in the chemical environment; NBR swelled in the benzene vapor (about 20% volume expansion) and the seal ring was extruded from its groove and cracked. Meanwhile the mineral base oil in the lithium grease also swelled the NBR slightly (about 5%); combined with the chemical-vapor swelling the total expansion reached 25%, exceeding the NBR limit (about 15%).
① In chemical environments the seal ring material should be FKM (fluoroelastomer, chemically resistant)\n② FKM's resistance to benzene-type vapor is 10× that of NBR\n③ Use a perfluoropolyether (PFPE) grease (chemically inert, does not react with chemical gases)\n④ Compatibility test of seal ring versus grease (immersion test, 70℃×168h)\n⑤ Seal replacement interval: NBR 1 month → FKM 6 months
FT_11 Ball Screw Selection