E41-517 · Linear Guide Selection · Spalling Around Linear Guide Base Bolt Holes · ★★★
After the linear guide mounting bolts were tightened, the cast iron base around the M12 bolt holes spalled (chips about 2×3mm), and the guide could no longer sit flat on the base.
When the guide bolt (torque 80Nm) is tightened in the M12 tapped hole of the cast iron base (HT300), the axial force of the bolt (about 25kN) is transferred from the bolt head through the washer (Φ20mm) into the base. The contact stress at the washer is σ_c=F/A=25000/(π×0.01²)≈79.6MPa. The compressive strength of HT300 is about 600MPa, so 79.6MPa is far below the compressive strength. However, the brittleness of cast iron causes cracking under local high stress (at the edge). The cross-section at the bolt hole edge (only 5mm from the edge of the base) is weak, and under the 25kN force the shear stress is τ=F/A=25000/(π×0.02×0.005)=79.6MPa. The shear strength of cast iron is about 200MPa, so 79.6MPa is within the safe range, but castings contain microscopic porosity and residual stress from casting (about 100MPa); combined with 79.6MPa this approaches the shear strength and the hole edge spalls.
1) Minimum distance from the bolt hole to the edge of the base ≥1.5d (d = bolt diameter);
2) Use a large-diameter washer (Φ28mm, reducing the contact stress to 40MPa);
3) Reduce the bolt tightening torque to the standard value (M12 torque 60~80Nm);
4) Inspect the hole edges for chipping after machining the bolt holes in the cast iron base;
5) Repair the chipped area: fill with epoxy resin and grind flat.
FT_10_Linear Guide Selection