E41-518 · Linear Guide Selection · Contamination Wear of Balls in the Linear Guide Carriage · ★★★
After one year of service the running resistance of the linear guide carriage increased unevenly from 50N to 80~120N over the full stroke. On disassembly pitted wear was found on the ball surfaces.
The balls inside the carriage (GCr15, 3.969mm) suffered abrasive wear once the grease was contaminated with foreign matter. The source of the contamination was airborne dust on the guide surface (about 5mg/m³) entering through the wiper seals of the carriage, forming an abrasive paste in the grease. The hard particles in the paste (SiO₂, hardness HV1000) produced three-body abrasion between the balls and the raceways. Pits appeared on the ball surfaces (diameter about 0.05mm, depth about 0.002mm), and the wear reduced the ball diameter by about 0.001mm. With the reduced ball diameter the preload fell from the ZA grade (about 2% of rated dynamic load) to about 1%, the clearance between carriage and guide increased, and the running resistance variation grew. The resistance is uneven because the wear is uneven (some regions wear more severely), so the resistance changes as the carriage travels over regions of differing wear.
1) Change the carriage grease regularly (every 6 months, clean out the old grease and add new grease);
2) Keep the guide surface clean (wipe the guide surface monthly with a lint-free cloth and kerosene);
3) Strengthen dust protection for the guide (fit a dust cover or an air curtain);
4) Select a self-lubricating carriage (large grease capacity, longer service interval);
5) Replace the carriage when the ball wear is serious (the balls cannot be replaced individually).