E41-522 · Linear Guide Selection · Hard Particles Embedded in the Guide Surface · ★★★★
Hard particles (weld spatter, hardness HV800) were pressed into the guide surface, forming scratches about 0.01mm deep, and the carriage produced a knocking noise when passing over the scratches.
During welding repair on the machine, welding was carried out near the linear guide and spatter (flux plus metal droplets, particle size 0.5~2mm) splashed onto the guide surface. As the carriage passed, the spatter was pressed into the raceway surface of the guide (hardness HRC60 ≈ HV700; the spatter is about HV800, harder than the guide itself). Once pressed in, the spatter produced indentations and scratches on the raceway surface (depth about 0.01mm, length about 3mm). When the carriage balls passed over the scratches they suffered an impact (acceleration about 2g) and a knocking sound was produced. On each pass over the scratches the contact stress on the balls doubles (stress concentration at the scratch edge) and after long-term running fatigue spalling develops in that region.
1) When welding near the linear guide the guide must be covered with protection (asbestos cloth + steel plate);
2) After welding, inspect the guide surface (visual inspection with a magnifier for spatter);
3) If spatter has been pressed in, gently grind away the raised spots and burrs with an oil stone;
4) Deep scratches (>0.01mm) require rail replacement (they cannot be repaired);
5) Check the balls for damage after the carriage has passed over the noisy region.
FT_10_Linear Guide Selection