E41-554 · Bearing Selection · Blocked Bearing Lubrication Line Starving the Bearing · ★★★★
After two years of running the lubrication line to the gearbox bearings became blocked and the bearings ran without oil (about 2h); the raceways overheated and turned blue (tempered colour).
The lubrication line (copper tube of bore Φ6mm, length 500mm) became blocked after two years of gearbox operation by oil sludge and wear particles (size about 0.1mm). The sludge consists of oxidation products of the lubricant (gum, about 30%) + gear wear debris (Fe, about 50%) + external dust (SiO₂, about 20%). The deposition rate in the line is about 0.01mm per month, so after two years the deposit layer is about 0.25mm thick and the effective bore of the Φ6mm line shrinks from Φ6mm to Φ5.5mm (flow area reduced by 16%), with the flow falling from 1L/min to about 0.5L/min (a 50% reduction). With the bearing oil supply reduced from 1L/min to 0.5L/min both the cooling and the lubrication of the bearing were inadequate. Running without oil for about 2h the bearing temperature rose from 45℃ to 120℃ and a blue tempered colour appeared on the raceway surface (indicating a temperature above 300℃). After tempering the raceway hardness fell from HRC62 to about HRC50 and the raceway developed plastic deformation.
1) Clean the lubrication line at regular intervals (every 2 years, flush with cleaning oil and blow through with compressed air);
2) Fit an oil flow indicator in the line (to observe the flow and act promptly when it drops);
3) Test and change the gearbox oil at regular intervals (sample every 6 months, change the oil when the Fe content exceeds 500ppm);
4) Fit a filter in the line (filter rating ≤25μm) to protect the bearing oil line;
5) Increase the line diameter: Φ6 → Φ8mm (a greater deposit tolerance, longer time before blockage).
FT_23_Bearing Selection Standards