E41-553 · Bearing Selection · Thermal Expansion of the Bearing Lock Nut Changing the Preload · ★★★★
After one hour of running (a spindle temperature rise of 40℃) the preload of the lock nut (M50×1.5) on the machine tool spindle bearing rose from 800N to 1200N and the bearing temperature rose further to 70℃.
The lock nut (45 steel, M50×1.5) expands by ΔD=α×D×ΔT=12×10⁻⁶×50×40=0.024mm at a temperature rise of 40℃. The nut bore grows by 0.024mm, but the spindle (40Cr, α=12×10⁻⁶/℃) expands by the same amount (the linear expansion coefficients are the same), so the radial expansion is consistent and has no effect. However, the axial expansion of the lock nut is ΔL=α×L×ΔT=12×10⁻⁶×8×40=0.0038mm (nut thickness 8mm). The 0.0038mm axial expansion increases the preload deformation of the bearing, raising the preload from 800N to 1200N (a 50% increase). The excessive preload increases bearing friction (heat generation up by about 30W), the temperature rises further to 70℃ and a positive feedback loop forms (preload rises → heat generation rises → temperature rises → preload rises further). In the end the bearing temperature stabilises at 70℃ (25℃ above the normal 45℃) and the grease life falls from 5000h to about 1000h.
1) Lock nut material for the spindle bearing: 45 steel → Invar (Fe-Ni alloy, α≈1×10⁻⁶/℃, thermal expansion one twelfth of steel);
2) Or use spring preload (constant-pressure preload, the spring compensating for thermal expansion so the preload stays constant);
3) Set the lock nut tightening torque at cold state to 80% of the standard value (it automatically rises to the standard value when hot);
4) Match the spindle material to the nut material (select materials with the same linear expansion coefficient);
5) Pre-warm the spindle (run at low speed empty for 30min before the load so that the thermal expansion stabilises, then adjust the preload).
FT_23_Bearing Selection Standards