Wrong Bearing Housing Material Causes Electrochemical Corrosion (Chemical Plant Agitator Bearing)

E41-582 · Bearing Selection · Chemical Plant Agitator Bearing Housing Corrosion · ★★★★

Problem Symptom

The bearing housing (cast iron HT200) of an agitator in a chemical plant showed severe corrosion on the fit surface between the bearing outer ring and the housing after 45 days; the housing bore was corroded from Φ100mm to Φ100.3mm and the bearing outer ring became loose.

Root Cause

The cast iron housing (HT200) is exposed to corrosive gas in the chemical plant environment (containing Cl₂ at about 5ppm). Cl₂ and the graphite in the cast iron form a galvanic cell (graphite as the cathode, ferrite as the anode), with an electrochemical corrosion rate of about 0.2mm per year (in a 5ppm Cl₂ environment). The actual corrosion was 0.3mm in 45 days (annualised to 2.4mm per year), 12 times the expected rate. The reason is that the housing surface carries machining burrs (Ra3.2μm), Cl₂ concentrates at the burrs (local concentration up to 50ppm) and, in addition, the housing contacts the stainless steel agitator shell (stainless steel and cast iron form a galvanic couple), which accelerates galvanic corrosion. The potential difference between the bearing outer ring (GCr15 bearing steel, chrome plated) and the cast iron housing is about 0.5V, so in the presence of a conducting medium (corrosive condensation) a galvanic current forms and the iron housing, acting as the anode, corrodes rapidly.

Correct Solution

1) In chemical environments the bearing housing should be stainless steel (316L) or engineering plastic (PTFE/PEEK);
2) Avoid contact between dissimilar metals (where stainless steel contacts cast iron the cast iron acts as the anode and corrodes faster);
3) Coat the contact surface between the housing and the bearing outer ring with anti-rust oil or conductive grease (reducing the galvanic effect);
4) Check the housing bore diameter at regular intervals (twice a year, replace promptly if corrosion is found);
5) Fit a sealed shroud to isolate the corrosive gas (sealed with a PTFE bellows).

Checklist

References