E41-436 · Cylinder and Hydraulic Selection · Cylinder Magnetic-Ring Demagnetization · ★★★
A cylinder in a high-temperature environment (80℃) lost its magnetic-switch signal after 6 months of use; replacing the switch did not help. Disassembly found the piston magnet ring had demagnetized.
The magnet ring (ferrite permanent-magnet material, remanence Br = 0.4 T) mounted on the cylinder piston gradually demagnetizes during long-term work at 80℃. The ferrite Curie temperature is about 450℃, but its irreversible demagnetization rate at 80℃ is about 5%/year. Over 6 months cumulative demagnetization is about 2.5%, dropping remanence to about 0.39 T. After a 2.5% drop in flux density, the magnetic switch (reed switch) trigger distance falls from 5 mm to about 3.5 mm (a 30% reduction). At installation the switch-to-cylinder gap was 4 mm; after demagnetization the flux is insufficient to trigger the switch and the signal is lost. Replacing the switch is ineffective (the problem is the ring, not the switch). Ferrite ring demagnetization at high temperature is permanent (irreversible).
① High-temperature environment (> 60℃) should use rare-earth permanent-magnet ring (NdFeB, Br = 1.2 T, temperature rating 150℃)\n② NdFeB irreversible demagnetization rate at 80℃ < 0.5%/year\n③ When installing magnetic switch, allow demagnetization margin in spacing to cylinder (install spacing = trigger distance × 0.7)\n④ After demagnetization, replace the piston assembly with magnet ring (cannot be re-magnetized)\n⑤ Or switch to Hall sensor (lower magnetic-field requirement than reed switch)
FT_31_Pneumatic System Design