Knowledge Base › Selection Error Cases › Poor scraping of plain-bearing shells leading to local contact overheating (large mill bearing shell)

Poor scraping of plain-bearing shells leading to local contact overheating (large mill bearing shell)

E41-308 · Other Selection · Large Mill Plain Bearing · ★★★★

Problem Description

During operation, the bearing shell temperature of a large ball-mill plain bearing (Φ1200mm) reached 75℃ (allowable ≤55℃); on shutdown inspection the bearing-shell contact spots were only about 40%.

Root Cause

Babbitt-metal bearing shells of plain bearings must be hand-scraped during installation, requiring ≥20 contact spots per 25×25mm². However, this bearing shell was scraped hastily by maintenance personnel, giving only 10~15 spots per 25×25mm² and about 40% contact area. The local contact zones were overloaded: contact stress σ_c=F/A=500kN/(π×0.6×0.4×0.4)=1657kPa (load 500kN, bearing-shell area about 0.75m²), and the oil-film thickness in the contact zones was h_min≤0.5μm (normally ≥3μm). Under boundary lubrication, the local friction coefficient rose from 0.005 to 0.05, heat generation increased 10 times, and the local temperature rise reached 50℃. The high temperature softened the Babbitt metal (melting point about 240℃, strength dropping 50% at 125℃), scored the bearing-shell surface, and let wear debris enter the oil circulation.

Corrective Solution

① Scraping standard for large plain bearings: ≥20 contact spots per 25×25mm², contact area ≥80%\n② Scraping method: first use red lead powder to reveal the high spots→remove the high spots with a scraper→repeat until the standard is met\n③ After installation, perform a barring check: manual barring should show no sticking\n④ After loading, run in: increase the load gradually, by 25% every 8h\n⑤ Check the bearing-shell temperature periodically (record every 2h, temperature difference ≤5℃)

Checklist

Reference

FT_Machine Design Handbook

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL