E41-472 · Other Selection · Rotary Joint Seal-ring Wear · ★★★★
The rotary joint of a rotary kiln feed pipe (carrying cooling water, speed 5 rpm, pressure 0.3 MPa) leaked at the seal ring after 1 year; cooling water splashed onto hot material, producing steam.
The rotary joint seal ring (silicon carbide/graphite friction pair) wears during long-term low-speed rotation. The mechanical seal of a silicon carbide ring (hardness HV2500) against a graphite ring (hardness HB80) has friction coefficient about 0.05 at 5 rpm and seal-face contact pressure about 0.3 MPa. Over 1 year cumulative rotation about 2.6×10⁶ rev (5 rpm×60 min×24 h×365 days = 2.6×10⁶ rev); silicon carbide ring wears about 0.002 mm, graphite ring about 0.2 mm. After wear the seal-face flatness degrades from 0.5 μm to 2 μm and clearance increases. Cooling water (0.3 MPa) leaks through the enlarged clearance. Leakage Q ∝ h³ (h = seal clearance); clearance from 0.5 μm to 2 μm (4×) raises leakage 64×. Daily water loss about 20 L. Reduced cooling water causes insufficient cooling of the feed pipe, and high temperature (about 800 ℃) burns out the feed pipe.
① Replace the rotary joint seal pair periodically (1 year).\n② Use a long-life seal pair (tungsten carbide/silicon carbide, 5× wear resistance).\n③ Add filtration to cooling water (accuracy ≤100 μm, prevent impurities wearing the seal face).\n④ Add leakage detection (drop sensor; stop and replace on detecting leakage).\n⑤ Cool/flush the seal face (flush with cooling water to carry away friction heat and impurities).
FT_Machine Design Handbook