E41-757 · Other Selection Topics · High Temperature Sight Glass Rupture · ★★★★
The sight glass of a reaction vessel (tempered glass, diameter Φ120mm, thickness 12mm) suddenly ruptured during use and the vessel contents sprayed out.
The sight glass operates at 200℃ and 0.5MPa. Tempered glass (soda-lime silicate glass) has an allowable working temperature ≤150℃ (at high temperature the tempering stress relaxes and the strength falls from 120MPa to 60MPa). At 200℃ the tempering stress has almost completely relaxed and the glass has become ordinary annealed glass (strength 30MPa). The pressure on the glass is σ=K×P×D²/(4×t²)=0.75×0.5×120²/(4×12²)=0.75×0.5×14400/(576)=9.375MPa (K being the support coefficient 0.75). 9.375MPa > the 30MPa strength of annealed glass, a safety factor of 3.2, which in theory is safe. However, the surface of the sight glass had micro-cracks (produced by the grinding wheel during machining, depth 0.05mm), giving a stress concentration factor Kt=5 and a local stress of 9.375×5=46.9MPa > 30MPa. After about 200 cumulative temperature cycles (200℃ → ambient → 200℃) the cracks propagated and the glass ruptured. The correct material choice is borosilicate glass (rated to 300℃) or sapphire glass (rated to 1000℃).
1) Re-check all the parameters against the correct selection specification;
2) Confirm that the duty load, environment and life all meet the design requirements;
3) Select a reliable brand and a suitable model;
4) Verify the installation and operating conditions;
5) Inspect and maintain the equipment at regular intervals after commissioning.
FT_Mechanical Design Handbook