E41-777 · Other Selection · Nameplate Unreadable · ★★
The outdoor equipment aluminum nameplate (anodized) oxidized severely after 2 years of use, and the engraved text became blurry and unreadable.
The anodized film (about 10 μm thick) has a weathering life of about 3–5 years outdoors (coastal, high salt-spray). But the nameplate engraving depth is only 0.3 mm (laser engraving); after 2 years of wind, rain, and UV the oxide film partially spalled and the engraving edges wore → blurred. Correct material: stainless steel nameplate (304, thickness 0.5 mm) plus laser engraving (depth ≥ 0.5 mm) or electrochemical etching (depth ≥ 0.3 mm).
① Recheck all parameters per correct selection specifications
② Confirm that operating loads, environment, and service life all meet design requirements
③ Select reliable brands and appropriate models
④ Verify installation and operating conditions
⑤ Perform periodic inspection and maintenance after commissioning
FT_Machine Design Handbook