E41-804 · Other Selection · Welding Distortion · ★★★
The equipment base (channel steel + steel plate welded structure, 3 m long, 1.5 m wide) developed wavy distortion after welding (flatness 5 mm, requirement ≤ 1 mm).
No anti-distortion measures were taken during base welding, and the welding sequence was unreasonable (long welds welded before short welds). Weld shrinkage: each fillet weld (leg 8 mm) shrinks about 0.8 mm/m transversely and about 0.5 mm/m longitudinally. The base has a total weld length of about 12 m, so total shrinkage is about 12×0.8 = 9.6 mm (transverse) + 12×0.5 = 6 mm (longitudinal); the uneven shrinkage caused wavy distortion (deformation about 5 mm). The welding residual stress (about 150 MPa) slowly released during natural aging, further aggravating the distortion. It should instead be stress-relief annealed after welding (600 °C × 2 h), or vibration aging should be used to remove residual stress.
① Recheck all parameters per correct selection specifications
② Confirm that operating loads, environment, and service life all meet design requirements
③ Select reliable brands and appropriate models
④ Verify installation and operating conditions
⑤ Perform periodic inspection and maintenance after commissioning
FT_Machine Design Handbook