Knowledge Base › Selection Error Cases › Lack of penetration caused by an undersized groove angle on a welded part (welding defect)

Lack of penetration caused by an undersized groove angle on a welded part (welding defect)

E41-827 · Other Selection · Weld Lack of Penetration · ★★★★

Problem Description

An X-ray inspection of the thick-plate (20 mm) butt weld found a lack-of-penetration defect (unfused at the weld root, depth about 5 mm).

Root Cause

A 20 mm thick plate was prepared with a single-V groove (groove angle 30°, root face 2 mm) for manual arc welding. The 30° groove angle was too small (recommended 45–60°); the electrode (Φ3.2 mm) could hardly reach the groove root, and the arc could not melt the base metal on both sides of the groove root. The 2 mm root face was not fully melted during the root pass, leaving about 1.5 mm of lack of fusion. The weld's effective load-bearing section dropped from 20 mm to 15 mm (a 25% loss), and under load stress cracking may initiate from the defect.

Corrective Solution

① Recheck all parameters per correct selection specifications
② Confirm that operating loads, environment, and service life all meet design requirements
③ Select reliable brands and appropriate models
④ Verify installation and operating conditions
⑤ Perform periodic inspection and maintenance after commissioning

Checklist

Reference

FT_Machine Design Handbook

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL