Gear tooth bending fatigue fracture caused by an undersized module (reducer high-speed stage gear)

E41-611 · Gear Drive Selection · Reducer High-Speed Stage Gear · ★★★★

Problem Description

The reducer high-speed stage gear (Z1 = 23, Z2 = 87, m = 3 mm) suffered tooth fracture after 4 months of operation; the fracture was at the tooth root and showed fatigue-fracture characteristics.

Root Cause

The gear module m = 3 mm was chosen by an empirical formula (P = 15 kW, n1 = 1450 rpm). Root bending stress calculation: σ_F = F_t×Y_F×Y_S×Y_ε/(b×m) = 2970×2.52×1.62×0.7/(56×3) = 49.5 MPa (F_t = 2T/d = 2×98800/66.5 = 2970 N, Y_F = 2.52, Y_S = 1.62, b = 56 mm). For a quenched-and-tempered 40Cr gear (tooth surface hardness HB280), the allowable bending stress [σ_F] = σ_Flim×Y_N/S_F = 350×0.9/1.25 = 252 MPa. 49.5 << 252, safety factor 5.1, so the tooth should not break. Recalculation showed the actual load T = 9550×P/n×K = 9550×15/1450×2.5 = 247 N·m (K = 2.5 is the application factor plus dynamic factor), actual F_t = 2×247000/66.5 = 7429 N, σ_F = 7429×2.52×1.62×0.7/(56×3) = 123.7 MPa. Still below 252 MPa. The tooth broke because the root fillet was poorly machined (after hob wear, a R0.1 mm sharp corner replaced the R0.4 mm fillet), raising the stress concentration factor from 1.6 to 2.8; actual stress σ_F = 123.7×2.8/1.6 = 216.5 MPa, and with impact load (actual K = 3.0), σ_F_peak = 216.5×3/2.5 = 259.8 MPa > 252 MPa, so fatigue cracks initiated at the root → propagated → tooth fracture.

Corrective Solution

① The gear module selection should verify root bending strength (including application factor K_A and dynamic factor K_V)\n② The hob should be inspected periodically for wear (root fillet R ≥ 0.38 m)\n③ The root fillet radius should be as large as possible (R ≥ 0.4 m recommended)\n④ Root shot peening (improves fatigue strength 30–50%)\n⑤ Change gear material to 42CrMo (allowable bending stress raised to 400 MPa)

Checklist

Reference

FT_Gear Transmission Design