E41-988 · Gear Drive Selection · Heat-treated Gear · ★★
A gear distorted 0.08 mm during quenching; assembly jammed, noise appeared, and it was scrapped.
First, quenching distortion skewed the tooth profile/lead, causing interference and jamming during assembly. Second, noise. Root cause: distortion.
① Control distortion in heat treatment (preheating / step quenching)
② Leave grinding allowance and precision-grind the tooth profile
③ Check the distortion ≤ 0.02
④ Choose a stable process
⑤ Do not assemble with excessive distortion
⑥ Measure tooth profile
⑦ If it jams, check the profile
FT_Gear Transmission Design