E41-645 · Belt Drive Selection · Pulley Groove Wear · ★★★
A belt drive (7 B-type belts, 37 kW) began slipping frequently after 1 year in service, and it still slipped after the belts were replaced. Inspection found the pulley grooves worn 1.5 mm deep.
The grooves of the cast-iron (HT200) pulley were worn by the belt over long service. The standard groove depth is 12 mm (B-type belt), but after 1 year the measured depth was 10.5 mm (1.5 mm of wear), and the groove angle had opened from the standard 36° to 38°. In a new groove the belt contacts the groove walls normally at a depth of 8~10 mm; after wear the belt sinks to a deeper position (about 10.5 mm from the groove mouth), the belt's outer diameter shrinks (effective diameter reduced from Φ200 mm to Φ197 mm), and the wrap angle decreases. In the smaller-diameter groove the belt's bending stress rises (σ_b=2×E×h/d=2×8×4/197≈0.325 MPa versus the normal 0.3 MPa—a minor effect). The key point is that the belt's contact area in the worn groove is reduced (the worn walls widen, changing the belt-wall contact from surface contact to line contact), lowering friction. The effective friction coefficient drops from μ=0.3 to μ=0.2, cutting transmission capacity by 33%. The capacity of the 7 B-type belts drops to 22.5 kW×0.7 (after wear)=15.75 kW, far below 37 kW, causing severe slipping.
① Pulley-groove wear inspection: measure groove width and angle with a pulley groove gauge\n② The standard groove width for a B-type belt is 17 mm (at the mouth); transmission efficiency suffers once wear pushes it >17.5 mm\n③ Replace the pulley when its grooves wear (wear >1 mm or service >2 years)\n④ Use a cast-iron pulley (more wear-resistant than a stamped steel pulley)\n⑤ High-frequency-harden the pulley's working face (HRC45~50, tripling life)
FT_Belt & Chain Drive Design