E41-844 · Belt Drive Selection · Hydraulic Gate Hoist · ★★
On an outdoor gate hoist (5.5 kW) the belt was exposed to sunlight year-round; after 2 years the surface cracked and the tensile strength fell sharply, and during the flood season the hoist failed, nearly flooding the land.
First, the antioxidants in standard rubber give only limited UV protection; UV broke the molecular chains in the surface rubber and caused ozone cracking (cracks running perpendicular to the load direction). Second, the crack depth grew about 1 mm per year and reached 2 mm in 2 years, penetrating the top rubber to the cords and cutting strength by 50%. Third, the cracking let the belt take up moisture and made it brittle in winter; at a peak hoisting torque of 1.8T it simply snapped. Root cause: a non-UV-resistant belt was chosen for outdoor use.
① For long-term outdoor exposure a UV-resistant belt must be used (CR or EPDM containing carbon black / anti-ozone wax)
② State the outdoor service conditions in the selection and choose the material from the weathering-resistance table
③ Add a sunshade or house the drive indoors to reduce direct sunlight
④ Inspect the surface for cracking annually; replace the belt once cracks reach the cords
⑤ Fit the gate hoist with a manual emergency mechanism to prevent flooding if the belt breaks
⑥ Standard light-colored / non-UV-resistant belts are forbidden outdoors
⑦ Carry out a dedicated inspection before the flood season