On a label printer (0.4 kW) the timing belt's back rubber cracked longitudinally; the teeth gradually spalled and the label feed became misaligned, scrapping about 2000 labels per day.
First, back-rubber cracking usually comes from the belt back being reverse-bent for long periods (tensioner diameter too small, d_t = 8 mm < the 12 mm minimum), over-fatiguing the back rubber in tension. Second, the bond strength between the back rubber and the cord is τ_b ≈ 3 MPa, while the reverse-bending stress σ_b' = E·t/d_t = 200·1/8 = 25 MPa > τ_b, debonding the interface. Third, once debonded the tooth roots lose the constraint of the back rubber, and meshing impacts spall the teeth and push the label-feed distance error beyond ±0.5 mm. Root cause: a tensioner diameter too small, fatiguing the back rubber.
① The timing-belt tensioner diameter must be ≥ the profile minimum (T5 ≥ 10 mm, T10 ≥ 15 mm); reverse bending over too small a pulley is forbidden
② Place the tensioner on the slack side to avoid sharp reverse bending of the belt back
③ At selection, check the back-rubber bending stress σ_b' = E·t/d_t ≤ τ_b
④ Switch to glass-fiber / aramid cord belts, whose stronger back-rubber bond resists spalling
⑤ Inspect the back rubber for cracks quarterly and replace the belt early
⑥ Tensioner diameters below the profile minimum are forbidden
⑦ If the label-feed accuracy drifts out of tolerance, inspect the belt back at once