Weld slag entering the system caused by improper hydraulic pipe welding

E41-688 · Hydraulic Component Selection · Pipe Welding Contamination · ★★★★

Problem Description

During commissioning of a newly installed hydraulic system the directional valve seized, and weld slag was found inside the spool.

Root Cause

The pipes were manually arc-welded without a TIG root pass, and uncleaned weld slag entered the system and jammed the spool.

Corrective Solution

① Use a TIG root pass for pipe welding
② After welding, pickle + passivate + flush in circulation until NAS ≤ 9
③ Install a temporary filter circuit before commissioning

Checklist

Reference

FT_Hydraulic & Pneumatic Design