E41-891 · Seal Component Selection · Process Pipe Flange · ★★★
One pipe flange bolts were not tightened to torque (only hand-tight); at operating temperature the flange opened, the gasket blew out, and medium sprayed out.
First, flange face pressure y must be ≥ gasket seating stress y_p (asbestos-rubber y≈11 MPa); insufficient torque leaves y<y_p and the gasket not compacted. Second, heating stretches bolts and drops preload; flange opening gap > gasket rebound → leak. Third, the gasket blew out and nearly injured someone. Root cause: insufficient torque + no hot tightening.
① Flange bolts must be tightened to the torque table (e.g. M20-8.8 ≈300 N·m) in a diagonal cross pattern
② For heated service, re-tighten hot (hot bolt-up)
③ Gasket seating stress y must be ≥y_p (per gasket type)
④ Use a torque wrench; do not rely on feel
⑤ Use spiral-wound gaskets + high torque on high-temperature flanges
⑥ Do not hand-tighten only
⑦ Check for no leakage on commissioning
FT_Seal Spring Design