One high-pressure vessel (40 MPa) used O-ring compression of 40%; the ring flattened with permanent set, and lost sealing on reassembly, leaking.
First, δ=40% far exceeds the static maximum 25%; rubber molecular chains slip irreversibly, ε_c>30%. Second, after unloading the ring does not rebound and the cross-section is flat; on reinstall the gap > rebound → leak. Third, high-pressure leakage hazard. Root cause: over-compression.
① Static seal compression ≤25% (high pressure take 15–20%)
② Add backup rings at high pressure to prevent extrusion and limit compression
③ Select low-ε_c material (FKM)
④ Design groove depth to the δ upper limit
⑤ Do not use δ>25%
⑥ Periodically check for flat cross-section
⑦ Check rebound on disassembly