Too Small Fillet Radius at the Spline Tooth Root Causes Fatigue Fracture of the Spline Shaft

E42-107 · Fatigue Fracture · Construction Machine Travel Gearbox · ★★★

Problem Symptom

Fatigue fracture at the spline tooth root after 2600 hours of running, affecting 3 units in a batch

Root Cause

[Tooth Root Bending Stress] The spline transmits T=1200N·m with z=14 teeth and module m=3, so the tooth root bending stress σ=Ft/(bmY)≈180MPa; the root fillet R=0.3 is too small, giving Kt=2.2.
[Fatigue Accumulation] The effective stress amplitude σa=180×2.2=396MPa exceeds the fatigue limit σ-1=320MPa of the spline steel, so the spline fractured after N≈2.6e6 cycles (2600 hours).
[Design Omission] The spline tooth root was not filleted and strengthened, and the fatigue was not checked.

Correct Solution

1) Increase the tooth root fillet to R=0.8 and grind the teeth;
2) Check the spline fatigue by finite element to ≥1e7 cycles;
3) Carburise and quench the surface to raise hardness;
4) Reduce the transmitted torque or increase the module;
5) Change to an involute spline to reduce the stress concentration;
6) Keep the assembly coaxiality ≤0.02mm;
7) Perform flaw detection every 2000 running hours;
8) Include spline fatigue in design review.

Checklist

References

GB/T 3478 Cylindrical Involute Straight Splines

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »