E42-212 · Fatigue Fracture · Worm Gear Reducer · ★★★
After 1800h, 3 worm gear teeth fracture at root; tooth surface pitting.
[High Bending Stress] Worm gear tooth root thickness b=8mm; face width too narrow; bending σ=210MPa near limit. [Fatigue Tooth Break] Under alternating load, root crack propagates and breaks at 1800h. [Design Omission] Insufficient face width margin; material tin bronze too soft.
1. Increase worm gear face width from 40mm to 60mm.
2. Change material to aluminum bronze ZCuAl10 for higher strength.
3. Run-in worm and gear to contact ≥70%.
4. Install overload coupling on input side.
5. Switch to extreme-pressure worm gear oil.
6. Load after no-load run-in at shipment.
7. Open housing quarterly to inspect tooth surface.
8. Design load spectrum at 1.5x.
GB/T 10089-2018