E42-261 · Fatigue Fracture · JM5-Ton Hoisting Drum · ★★★
JM5 hoisting drum (Φ400×1000) circumferential crack at rope groove bottom 35mm long, depth half wall thickness (wall 25mm); rope break risk; 4 shutdown maintenance per month
[Stress Concentration] Rope groove bottom fillet r=2mm (should be ≥6mm); estimated by Kt=1+2√(h/r), Kt≈2.6; under wire rope squeeze force F=42kN, groove bottom nominal stress σn=F/(r·b)=42e3/(0.002×0.05)=420MPa.
[Fatigue Propagation] Actual stress σ=Kt·σn=2.6×420=1092MPa far exceeding groove steel allowable fatigue limit 260MPa; per Miner criterion life only 12,000 cycles (design ≥50,000); crack initiates at fillet root.
[Design Omission] Rope groove not roll-strengthened; fillet not selected per wire rope diameter; safety factor only 1.1 (should be ≥1.8); no fatigue strength check.
1) Increase rope groove fillet from r=2mm to r≥6mm and polish to Ra0.8;
2) Roll-strengthen groove bottom to create -300MPa surface compressive stress;
3) Increase drum wall thickness from 25mm to 32mm; change material to Q345B;
4) Select groove profile per rope diameter d; groove depth ≥1.5d, pitch ≥1.1d;
5) Limit working load to 80% rated (≤4t);
6) Monthly magnetic-particle inspect groove bottom and build crack ledger;
7) Install torque limiter for auto shutdown at 10% overload;
8) Mandatory drum replacement at 15,000 working cycles.
GB/T 5972-2016