Knowledge Base › Structural Design Error Case Study › Hoisting Wire Rope Fatigue Wire Breaks

Hoisting Wire Rope Fatigue Wire Breaks

E42-377 · Fatigue Fracture · Mine Hoisting Wire Rope · ★★★

Problem Description

Mine hoist rope (6×19) in service wire breaks exceed spec; rope replaced; 1 inspection per month

Root Cause

[Bending] Rope bends over head sheave; bending stress σ=480MPa exceeds fatigue.
[Wire Breaks] By L=CA²/d, life shortened.
[Design Omission] Head sheave diameter too small (d ratio 17); not lubricated; safety factor 1.3.

Corrective Solution

1) Raise head sheave diameter ratio to ≥40;
2) Periodic lubrication;
3) Select one size larger rope diameter;
4) Fatigue check;
5) Inspect wire breaks each shift;
6) Anti-rotation structure;
7) Limit speed;
8) Mandatory inspection at due date.

Checklist

Reference

GB/T 5972-2016