Knowledge Base › Structural Design Error Case Study › Excessive Weld Reinforcement Causing Weld Toe Stress Concentration Fatigue Source

Excessive Weld Reinforcement Causing Weld Toe Stress Concentration Fatigue Source

E42-162 · Welding Deformation and Defects · Mining Conveyor Middle Trough · ★★★

Problem Description

After 6 months operation, weld toe fatigue crack; propagates to base metal, chain breaks.

Root Cause

[Excessive Reinforcement] Fillet weld reinforcement h=4mm (should be ≤1.5); weld toe included angle 120°. [Stress Concentration] Weld toe K_t=2.5; pulsating load σ_max=210MPa. [Design Omission] Weld toe not ground; no TIG remelting; chain broke.

Corrective Solution

1. Control fillet weld reinforcement to ≤1.5mm.
2. Grind weld toe smooth R≥2mm.
3. TIG remelt weld toes at critical positions.
4. Weld profile per ISO5817 grade B.
5. Match consumable strength to base metal.
6. Raise flaw detection rate to 100%.
7. Ultrasonic impact strengthen fatigue-prone positions.
8. Shift-point inspection of weld toe cracks.

Checklist

Reference

GB/T 19869.1-2005

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »