Knowledge Base › Structural Design Error Case Study › Small Weld Groove Angle Causing Root Lack of Fusion

Small Weld Groove Angle Causing Root Lack of Fusion

E42-216 · Welding Deformation and Defects · Overhead Crane Box Girder · ★★★

Problem Description

Flaw detection found root lack of fusion in butt weld 80mm long; load capacity reduced.

Root Cause

[Groove Too Small] Single-V groove angle α=35° (should be 50°); root gap c=1mm; electrode cannot reach root. [Lack of Fusion] Arc fails to penetrate base metal; unbonded interface forms. [Design Omission] Groove taken at minimum angle; no welding procedure qualification.

Corrective Solution

1. Change groove angle to 55°; land 2mm; gap 3mm.
2. Perform welding procedure qualification (WPS) before welding.
3. Add backing strip at root to ensure back-side profile.
4. Layer welding with 4mm electrode diameter.
5. 100% UT inspection after welding.
6. Welders certified for the job.
7. Interpass temperature not exceeding 250℃.
8. Repair per NB/T standard.

Checklist

Reference

NB/T 47014-2011