Knowledge Base › Structural Design Error Case Study › Stainless Steel Welding Without Backing Gas Protection Causing Oxidation and Lack of Penetration

Stainless Steel Welding Without Backing Gas Protection Causing Oxidation and Lack of Penetration

E42-217 · Welding Deformation and Defects · Food-Grade Stainless Tank · ★★★

Problem Description

Inner pipe weld blackened; intergranular oxidation; leaks on hydrostatic test.

Root Cause

[Back-Side Oxidation] 304 pipe inner weld without argon backing; back-side chromium oxidized to Cr₂O₃; poor fusion. [Lack of Penetration Leak] Oxide layer impedes fusion; root micropores seep. [Design Omission] No backing gas per stainless welding code; no argon purge.

Corrective Solution

1. Purge pipe interior with argon backing, purity 99.99%.
2. Use ER308L low-C welding wire.
3. Control interpass temperature ≤150℃ to prevent sensitization.
4. Pickle and passivate after welding.
5. Perform penetrant testing with no leakage.
6. Welders hold special stainless certification.
7. Hydrostatic test at 1.5x hold pressure.
8. Clean oil from groove before each pass.

Checklist

Reference

GB/T 985.1-2008