E42-381 · Welding Deformation and Defects · φ1800 Air Tank Shell · ★★★
φ1800 air tank shell longitudinal seam angular misalignment E=8mm exceeds allowable 3; misaligned edge; leaks on pressure test; 2 units repaired per month
[Angular Misalignment] Single-side weld uneven shrinkage; angular misalignment E=8mm.
[Leak] Misaligned edge causes stress concentration crack.
[Design Omission] Welding sequence not controlled; no reverse deformation; safety factor 1.4.
1) Symmetric longitudinal seam welding to control angular misalignment ≤3;
2) Preset reverse deformation;
3) Rigid roller jig;
4) Round-up after welding;
5) RT inspect each seam;
6) Control misaligned edge ≤1.5;
7) Post-weld annealing;
8) Hydrostatic test each unit.
GB/T 150.4-2011