E42-382 · Welding Deformation and Defects · QD Crane Box Girder · ★★
QD crane box girder web plate waviness δ=6mm exceeds allowable 4; local dent; 2 units repaired per month
[Waviness] Welding compressive stress causes web plate buckling waves.
[Dent] Local warpage.
[Design Omission] No longitudinal stiffener; plate thickness too small; safety factor 1.4.
1) Add longitudinal stiffeners to web plate;
2) Upgrade plate thickness one grade;
3) Symmetric welding to control deformation;
4) Level after welding;
5) Measure waviness per girder;
6) Control stiffener spacing;
7) Post-weld annealing;
8) Periodic patrol.
GB/T 14405-2011