E42-383 · Welding Deformation and Defects · 5000m³ Oil Tank Bottom Plate · ★★
5000m³ oil tank bottom plate lap-joint angular distortion; local lift-up 5mm; water seepage; 1 spot repaired per month
[Angular Distortion] Lap weld shrinkage; edge lifts 5mm.
[Seepage] Lifted seam holds water and corrodes.
[Design Omission] No segmented back-step welding; no ballast weight; safety factor 1.4.
1) Segmented back-step welding;
2) Ballast weight over weld zone to prevent lift-up;
3) Control angular distortion ≤3;
4) Vacuum leak test after welding;
5) Inspect distortion per seam;
6) Thicken bottom plate;
7) Flaw detection after welding;
8) Periodic thickness measurement.
GB 50128-2014