E42-386 · Welding Deformation and Defects · Steel Pipe Truss Joint · ★★★
Steel pipe truss gusset plate lack of fusion 4mm deep; joint loose; 1 spot repaired per month
[Lack of Fusion] Small groove angle; low heat input; 4mm deep lack of fusion.
[Loose] Joint force transfer fails.
[Design Omission] Groove design wrong; no root gouging; safety factor 1.4.
1) Machine double-sided groove on gusset plate;
2) Gouge root and weld through-penetration;
3) Control heat input to mid-value;
4) UT inspection;
5) Inspect fusion per joint;
6) Reinforce with stiffener;
7) Post-weld annealing;
8) Load test.
GB 50017-2017