E42-387 · Welding Deformation and Defects · Glass-Lined Reactor Jacket · ★★★
Glass-lined reactor jacket circumferential seam leaks; media mix; 2 units repaired per month
[Leak] Jacket fillet weld not through-penetrated; bubbles on leak test.
[Media Mix] Medium seeps in.
[Design Omission] No helium leak test; wrong weld sequence; safety factor 1.4.
1) Through-penetrate jacket weld and helium test;
2) Post-weld 0.4MPa pneumatic test;
3) Grind fillet weld;
4) Weld sequence inside first then outside;
5) Pneumatic test each unit;
6) Material matching;
7) Post-weld annealing;
8) Periodic patrol.
HG/T 2370-2017