Pressure Vessel Nozzle Fillet Weld Crack

E42-462 · Welding Deformation and Defects · Pressure Vessel Nozzle · ★★★

Problem Description

Pressure vessel (φ2000) nozzle fillet weld crack 30mm long; leaks; 1 repair per month

Root Cause

[Fillet Weld] Nozzle corner stress concentration Kt=2.5; σ=160MPa.
[Crack] Welding residual + working stress crack.
[Design Omission] No NDT; no smooth transition; safety factor 1.3 (should be ≥3.0).

Corrective Solution

1) Corner R≥10mm smooth;
2) RT inspect after welding;
3) Preheat 150℃;
4) Increase fillet weld size;
5) Inspect cracks each unit;
6) Limit working pressure;
7) Upgrade material Q345R;
8) Periodic re-measurement.

Checklist

Reference

GB/T 150.4-2011

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL