Knowledge Base › Structural Design Error Case Study › Pressure Vessel Circumferential Seam Lack of Fusion

Pressure Vessel Circumferential Seam Lack of Fusion

E42-511 · Welding Deformation and Defects · Air Tank (φ1200) · ★★★

Problem Description

Circumferential seam X-ray found lack of fusion 120mm long; leaks on pressure test; 2 units scrapped per month

Root Cause

[Lack of Fusion] Current I=110A too low; small groove angle; insufficient penetration.
[Defect] Incomplete root gouging; slag inclusion.
[Design Omission] No welding parameters specified; no flaw detection; safety factor 1.2 (should be ≥2.0).

Corrective Solution

1) Raise current to 140A;
2) Change groove angle to 60°;
3) Gouge root before welding;
4) 100% RT inspection;
5) Visual inspection each shift;
6) Control interpass temperature;
7) Certified welders;
8) Periodic pressure test.

Checklist

Reference

GB/T 150.4-2011

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »