Knowledge Base › Structural Design Error Case Study › Truss Joint Weld Cold Crack

Truss Joint Weld Cold Crack

E42-512 · Welding Deformation and Defects · Steel Structure Truss · ★★

Problem Description

The fillet weld at the joint has hydrogen-induced cracks 80mm long, load capacity drops 30%; 3 locations reinforced per year

Root Cause

[Cold Crack] Hydrogen content H=8mL/100g, fast cooling, hardening.
[Stress] High restraint, no preheat.
[Design Omission] Hydrogen not controlled, no preheat; safety factor 1.3 (should be ≥2.0).

Corrective Solution

1) Dry electrodes at 350℃;
2) Preheat to 120℃ before welding;
3) Use low-hydrogen filler metal;
4) Slow cooling after welding;
5) Crack check each shift;
6) Stress-relief annealing;
7) Add ribs at joint;
8) Periodic NDE.

Checklist

Reference

GB/T 50661-2011