Worn Mould Dowel Pins on a Box Casting Cause Misalignment Out of Tolerance

E42-065 · Casting Defects · Box Casting HT200 · ★★

Problem Symptom

Misalignment 0.8mm, insufficient machining allowance

Root Cause

[Misalignment Amount] The upper mould is offset by 0.8mm because the mould dowel pins have worn from Φ12 to Φ12.5, giving excessive clearance.
[Misalignment] The parting-line misalignment makes the wall thickness differ by 1.6mm and leaves only 0.5mm of machining allowance on one side.
[Design Omission] The dowel pins were not replaced on schedule and no mould closing check was made, so the casting was scrapped.

Correct Solution

1) Replace the dowel pins periodically to maintain Φ12h7;
2) Check the misalignment in full before closing, to ≤0.3mm;
3) Add dowel stops to prevent misassembly;
4) Increase the machining allowance to cover the misalignment;
5) Segregate and recast misaligned parts;
6) Calibrate the mould plate accuracy;
7) Section the first article to check wall thickness;
8) Include the mould closing check in the process.

Checklist

References

GB/T 6414-2017 Castings — Dimensional Tolerances

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL