Knowledge Base › Structural Design Error Case Study › Low Pouring Temperature on Thin-Wall Casting Causing Misrun and Missing Metal

Low Pouring Temperature on Thin-Wall Casting Causing Misrun and Missing Metal

E42-271 · Casting Defects · Thin-Wall Box · ★★

Problem Description

The thin-wall box (4mm wall) is unfilled at the far end with 3 spots of missing metal and incomplete outline; monthly scrap rate 12%

Root Cause

[Low Temperature] Pouring temperature 1280℃ (should be ≥1360℃); iron fluid fluidity insufficient; fill length reaches only 80% of wall length.
[Misrun] The far-end thin wall (4mm) freezes early and is unfilled with 3 spots of missing metal; minimum remaining wall thickness 1.5mm.
[Design Omission] Pouring temperature not raised, gating system not modified; process yield only 62% (should be ≥75%).

Corrective Solution

1) Raise pouring temperature to 1380±10℃;
2) Thicken thin sections to 6mm and add padding;
3) Add overflow/vent risers;
4) Raise pouring rate to 1.2kg/s;
5) Increase pattern draft to 3°;
6) Section-inspect the first piece of each batch;
7) Recheck gating system ratios;
8) Control molding sand moisture to 4%~5%.

Checklist

Reference

GB/T 9439-2010