Knowledge Base › Structural Design Error Case Study › Off-Set Ingate Causing Local Shrinkage Cavity at Heavy Section

Off-Set Ingate Causing Local Shrinkage Cavity at Heavy Section

E42-274 · Casting Defects · Gear Blank · ★★

Problem Description

The gear blank (Φ200) has a shrinkage cavity Φ10 at the heavy section, exposed after machining; 10 parts scrapped per month

Root Cause

[Off-Set Gate] The ingate is off-center and the heavy section (Φ80) is not aligned with the riser, blocking the feed channel.
[Shrinkage Cavity] Hot-spot shrinkage cavity Φ10, volume about 8cm³, exposed after machining and scrapped.
[Design Omission] Wrong gate layout, riser too small (volume only 1.2x the hot spot, should be ≥2.5x).

Corrective Solution

1) Align the ingate with the heavy-section riser;
2) Place an open riser on top of the heavy section;
3) Add chills to balance solidification;
4) Increase riser volume by 30% or more;
5) Check gating per mold;
6) UT inspect before machining;
7) Solidification process simulation;
8) Section the first piece to verify.

Checklist

Reference

GB/T 7233.1-2009