Knowledge Base › Structural Design Error Case Study › Core Chaplet Displacement Causing Uneven Wall Thickness and Leakage

Core Chaplet Displacement Causing Uneven Wall Thickness and Leakage

E42-273 · Casting Defects · Cylinder Block · ★★

Problem Description

The cylinder casting wall locally thins to 3mm (designed 6mm); leaks at 0.4MPa hydrostatic test; 15 parts scrapped per month

Root Cause

[Chaplet Displacement] The core support shifts 5mm; after solidification the local wall is only 3mm.
[Leakage] Porosity in the thin wall leaks at 0.4MPa hydrostatic test, sealing surface fails.
[Design Omission] Chaplets not fixed or verified; wall tolerance only ±2mm (should be ±0.8mm).

Corrective Solution

1) Add locating pins to fix the core and prevent shift;
2) Spot-weld or rivet chaplets;
3) Raise wall thickness to 8mm, uniformly distributed;
4) Add padding to prevent porosity;
5) Check core position per mold;
6) Hydrostatic-test each part at 0.6MPa;
7) Recheck pattern wall thickness;
8) X-ray sampling for porosity.

Checklist

Reference

GB/T 9439-2010

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL