Knowledge Base › Structural Design Error Case Study › Porosity at Main Journal of Crankshaft Blank

Porosity at Main Journal of Crankshaft Blank

E42-391 · Casting Defects · Ductile Iron Crankshaft Blank · ★★★

Problem Description

The ductile iron crankshaft main journal shows porosity Φ6 after machining and is scrapped; 3 shafts scrapped per month

Root Cause

[Porosity] The hot spot (Φ70) is not aligned with the riser; feeding insufficient.
[Scrap] Porosity exposed after machining.
[Design Omission] Riser too small, no chills; safety factor 1.4.

Corrective Solution

1) Place an open riser on top of the hot spot;
2) Add chills for balance;
3) Increase riser by 30%;
4) Optimize the gating system;
5) UT each shaft;
6) Process simulation;
7) Section the first piece;
8) Composition control.

Checklist

Reference

GB/T 1348-2019

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »