E42-392 · Casting Defects · Diesel Engine Cylinder Block · ★★★
The diesel engine cylinder block water jacket has sand holes Φ4, leaks at 0.3MPa hydrostatic test; 2 parts scrapped per month
[Sand Holes] Residual sand, local sand holes.
[Leakage] Water cavity penetrated.
[Design Omission] Uneven sand compaction, no sand removal; safety factor 1.4.
1) Keep sand compaction uniformly ≥85%;
2) Coat the water cavity;
3) Raise pouring temperature;
4) Hydrostatic-test each part;
5) X-ray sampling;
6) Sand removal process;
7) Add wall-thickness allowance;
8) Section the first piece.
GB/T 9439-2010