Knowledge Base › Structural Design Error Case Study › Missing Metal on Impeller Blades

Missing Metal on Impeller Blades

E42-397 · Casting Defects · Stainless Steel Centrifugal Impeller · ★★★

Problem Description

The stainless steel impeller blades (3mm thick) have missing metal and dynamic unbalance; 2 parts scrapped per month

Root Cause

[Missing Metal] Thin blade, incomplete filling, short 0.8mm.
[Unbalance] Mass offset.
[Design Omission] Pouring temperature not raised, not thickened; safety factor 1.4.

Corrective Solution

1) Thicken blades to 4mm;
2) Raise pouring temperature to 1480℃;
3) Provide feed risers;
4) Dynamic-balance each impeller;
5) X-ray sampling;
6) Airfoil template inspection;
7) Standardize weld repair;
8) Section the first piece.

Checklist

Reference

GB/T 5657-2013

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL