Knowledge Base › Structural Design Error Case Study › Cold Shuts on Flywheel Spokes

Cold Shuts on Flywheel Spokes

E42-396 · Casting Defects · Cast Iron Flywheel · ★★

Problem Description

The cast-iron flywheel spokes have cold shuts and reduced strength; 1 part scrapped per month

Root Cause

[Cold Shut] Two metal streams fail to fuse, leaving a cold-shut seam.
[Strength Loss] Weak section.
[Design Omission] Low pouring temperature, slow flow; safety factor 1.4.

Corrective Solution

1) Raise pouring temperature by 20℃;
2) Speed up pouring;
3) Thicken the spokes;
4) Provide overflow;
5) Magnetic particle test each batch;
6) Ultrasonic thickness measurement;
7) Dynamic balance;
8) Section the first piece.

Checklist

Reference

GB/T 9439-2010