Knowledge Base › Structural Design Error Case Study › Hot-Spot Shrinkage Cavity in Large Steel Casting

Hot-Spot Shrinkage Cavity in Large Steel Casting

E42-463 · Casting Defects · Large Steel Casting · ★★

Problem Description

The large steel casting (30t) has hot-spot shrinkage cavity φ40 with reduced mechanical properties; 1 part scrapped per month

Root Cause

[Hot Spot] The thick wall intersection solidifies slowly, leaving shrinkage cavity φ40.
[Porosity] Feeding insufficient.
[Design Omission] No risers, no chills; process yield only 55%.

Corrective Solution

1) Provide insulating risers;
2) Add chills at hot spots;
3) Design a necked-down riser neck;
4) Control pouring temperature to 1560℃;
5) NDE each piece;
6) Provide padding;
7) Limit wall-thickness difference;
8) Periodic re-measurement.

Checklist

Reference

GB/T 11352-2009