Graphite Flotation on Ductile Iron Casting

E42-464 · Casting Defects · Ductile Iron Casting · ★★

Problem Description

The ductile iron casting (QT450) has a graphite flotation layer 3mm thick with brittle surface layer; 4 parts scrapped per month

Root Cause

[Flotation] High carbon equivalent CE=4.7% and high pouring temperature 1420℃ cause graphite to float up in a 3mm layer.
[Brittle] Low surface-layer strength.
[Design Omission] CE not limited, pouring temperature not lowered; improper process.

Corrective Solution

1) Control CE to 4.3-4.5%;
2) Lower pouring temperature to ≤1380℃;
3) Add chills to promote solidification;
4) Vent the cavity;
5) Metallography each batch;
6) Clean the surface layer;
7) Limit wall thickness;
8) Periodic re-measurement.

Checklist

Reference

GB/T 1348-2009